MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SHIELD® 610 A/B Epoxy Conductive Coating
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: CHO-SHIELD® 610 A/B is a highly conductive, two-component silver-plated-copper filled epoxy coating for application to non-conductive plastic substrates, particularly those subject to hostile environmental conditions of abrasion, temperature extremes, high humidity, and salt fog corrosion. It dries to the touch in less than one hour with best performance attained by using one of two accelerated cure cycles.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 - 1.75 g/cc1.45 - 1.75 g/cc
Volatile Organic Compounds (VOC) Content 888 g/l888 g/l
Thickness 50.0 microns1.97 milRecommended
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.15 ohm<= 0.15 ohm2 mils thickness
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 121 °C
1.00 hour
@Temperature 250 °F
 120 min
@Temperature 24.0 °C
2.00 hour
@Temperature 75.2 °F
 240 min
@Temperature 79.0 °C
4.00 hour
@Temperature 174 °F
 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
Pot Life 480 min480 min
Working Life 480 min480 min
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
BinderEpoxy
ConsistencyMedium Fluid
Coverage453/gal@ 0.001 in thick
 718 sq. ft2/gal/mil thickness
Cross Hatch Adhesion5BASTM D3359-78 Method B)
FillerAg/Cu
High Temperature Test129240 hrs. @ 85°C, Initial Resistance
 151240 hrs. @ 85°C, Final Resistance
Humidity Test125240 hrs. @ 65°C and 85-95% RH, Initial Resistance
 125240 hrs. @ 65°C and 85-95% RH, Initial Resistance
Low Temperature Test133240 hrs. @ -40°C, Initial Resistance
 137240 hrs. @ -40°C, Final Resistance
Mix Ratio100:28
Salt Fog Test11996 hrs. Initial Resistance; ASTM B-117
 19696 hrs. Final Resistance; ASTM B-117
Suggested Spraying Viscosity #2 Zahn Cup19 - 27 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME229 / 130939

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.