Notes: Sarlink ME-2340B-02 BLK XRD1 is a high performance thermoplastic elastomer used in automotive applications including exterior trim and weatherstripping. Sarlink ME-2340B-02 BLK XRD1 is a low hardness, low density, light stabilized grade suitable for injection molding. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Filled; High Slip; Light Stabilized; Low Density; Low Fogging; Low Friction; Low Hardness; Low Specific Gravity; Lubricated; Medium Flow; Sunlight Resistant; UV Absorbing Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Grommets; Weatherstripping RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |