MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Inov Chem Donpipe 322 HCFC-141b Base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonPipe 322 is a kind of blend polyols with hcfc-141b as foaming agent, taking polyol as the main raw material, mixing with a special auxiliary. This material suitable for outer thermal insulation shells which are used for water, oil and gas pipelines. The polyurethane product prepared by reacting it with isocyanate has the following advantages:
-- good compressive strength and dimensional stability
-- high close-cell rate and good waterproof performance
-- good insulation performance

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 - 1.16 g/cc
Density 0.0250 - 0.0300 g/ccFree density, Manual Mix
 0.0250 - 0.0300 g/ccFree density, High Pressure
 >= 0.0500 g/ccMold density; GB/T 6343
Viscosity 200 - 400 cPDynamic
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.150 MPaGB/T 8813
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0220 W/m-K
@Temperature 10.0 °C
GB/T 3399
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CMaterial Temperature, Manual mix
 20.0 - 25.0 °CMaterial Temperature, High pressure
Cure Time 30.0 - 50.0 secTack free time, High pressure
 40.0 - 60.0 secTack free time, Manual Mix
Gel Time 0.300 - 0.670 minHigh Pressure
 0.500 - 0.830 minManual Mix
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow transparent viscous liquid
Closed-cell rate=90%GB/T 10799
Cream time6-12 secHigh Pressure
 7-15 secManual Mix
Dimensional stability=0.5%24h, -20?; GB/T8811
 =1.0%24h, 100?; GB/T8811
FlammabilityB3, B2, B1GB/T 8624
Hydroxyl value200-400 mgKOH/g
Recommended Ratio100:120-160DonPipe 322:Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM014 / 312543

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.