MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ME-2160B Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2160B series are general purpose thermoplastic elastomer designed for exterior automotive molding applications. Sarlink ME-2160B is a medium hardness, high density, filled grade having good UV resistance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Good Flexibility; Good Flow; Good Processability; Good Toughness; High Density; Medium Hardness; High Specific Gravity; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Viscosity 116 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ISO 11443
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 56ISO 868
Tensile Strength at Break 957 psiISO 37
Tensile Stress at Strain 189 psi
@Strain 100 %
ISO 37
Elongation at Break 870 %ISO 37
Compression Set 44 %ISO 868
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 329 - 347 °F
Middle Barrel Temperature 347 - 365 °F
Front Barrel Temperature 369 - 387 °F
Nozzle Temperature 369 - 387 °F
Melt Temperature 369 - 387 °F
Mold Temperature 68.0 - 104 °F
Injection Pressure 200 - 1000 psi
Back Pressure 24.9 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1052 / 237543

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.