MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Polyram PlusTek PD1002NT Nylon 12 for Extrusion
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: Medium viscosity Nylon 12 for extrusion application.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Moisture Absorption at Equilibrium 0.70 %50% RH; ISO 62
Water Absorption at Saturation 1.15 %ISO 62
Linear Mold Shrinkage 0.0080 - 0.0090 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPaISO 527
Elongation at Break 70 %ISO 527
Tensile Modulus 1100 MPaISO 527
Izod Impact, Unnotched (ISO) 8.00 kJ/m²ISO 180
Charpy Impact Unnotched NBISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Strength 32.0 kV/mmIEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 175 °CISO 11357
Maximum Service Temperature, Air 105 °CContinuous use
 150 °CShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75
Flammability, UL94 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Hippe PA 11 Nylon 11
Evonik VESTAMID® NRG 6001 PA 12
Evonik Trogamid® CX9710 Transparent Nylon
Evonik Trogamid® CX9701 Transparent Nylon

PPOLYR802 / 126601

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.