MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® RG-18108 NAT Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-18108 is a high performance thermoplastic elastomer, available in NAT and colors, intended for use in food contact applications. Monprene RG-18108 is a very soft, low density grade with good adhesion to PP and complies with various US FDA regulations and EU directives for food contact. This grade is suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Bondability; Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Processability; Halogen Free; High Elasticity; Low Density; Low Hardness; Low Specific Gravity; Lubricated

Uses: Flexible Grips; Non-specific Food Applications; Overmolding; Rubber Replacement; Seals; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.872 g/ccASTM D792
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 150 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8.0
@Time 5.00 sec
Injection Molded; ASTM D2240
 11
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 160 psiASTM D412
Elongation at Break 800 %Die C, 20 in/min; ASTM D412
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 300 - 340 °F
Middle Barrel Temperature 340 - 380 °F
Front Barrel Temperature 380 - 440 °F
Nozzle Temperature 380 - 440 °F
Melt Temperature 380 - 440 °F
Mold Temperature 70.0 - 125 °F
Back Pressure 50.0 - 100 psi
Cushion 0.140 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0933 / 237424

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.