MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Eccobond® A410-05P One-Component Thermally Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Emerson & Cuming A410-05P Eccobond® One-Component Thermally Conductive Epoxy Adhesive
High strength, aluminum filled, epoxy adhesive for bonding to most oily or other poorly prepared metal surfaces. Sag resistant. Excellent heat and chemical resistance. Recommended for bonding metal motor housings. Cure Type: Heat Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 4000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 hour
@Temperature 160 °C
 0.750 hour
@Temperature 120 °C
 
Descriptive Properties
ColorGrey
ViscosityThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive
Trelleborg Emerson & Cuming Eccobond® 59C One-Component Silver Filled Electrically Conductive Silicone Adhesive
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Trelleborg Emerson & Cuming Eccobond® 56C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Trelleborg Emerson & Cuming Eccobond® 285 Two-Component Thermally Conductive Epoxy Adhesive

PEMERS59 / 35751

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.