MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Premabraze 131 Gold Based Brazing Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes:

Applications:Premabraze 131 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well suited for brazing thin section, such as thin-wall tubing or electronic vacuum tubes. It has also been used extensively for nuclear power applications, except in high flux regions and in contact with such liquid metals as sodium and potassium.

Characteristics:Premabraze 131 wets a wide range of high temperature iron and nickel based alloys such as the stainless steels, A286, Inconel and Inconel X very well. It does not alloy excessively with these materials nor produce the severe intergranular penetration normally associated with the nickel based brazing alloys contained boron.

A minimum brazing temperature of 1800EF (980EC) is suggested for furnace brazing in hydrogen or dissociated ammonia having a -40EF dew point or drier on 300 and 400 series stainless steels which do not contain additions of Ti or Al.

Stainless steels of the 17-7 PH variety require dew points of -70EF or drier for furnace brazing.

Brazing is done in inert atmospheres or in vacuum.

For torch brazing, protection with Handy Hi-Temp Flux is recommended. Where base metals containing elements which produce refractory oxides are encountered, Handy Hi-Temp Flux Boron Modified will promote better wetting.

Joint clearances of 0.0015" - 0.003" are normally suggested.

Gold and nickel are completely soluble in all proportions at temperatures above 1490EF (810EC) and this specific composition (82% Au- 18% Ni) represents the minimum in this system so that the solidus (melting point) and the liquidus (flow point) are identical.

Normally, Premabraze 131 would not be used for joining copper based and silver based alloys. In addition to have a flow point very close to the melting point of silver, and above that of the silver-copper eutectic, it would alloy quite readily with copper based alloys.

Specifications:Premabraze 131 conforms to: AWS A5.8 BVAu-4, Grade 1

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 15.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 62000 psi
@Temperature 23.0 °C
Tensile Strength, Ultimate 20000 psi
@Temperature 871 °C
Type 304 Stainless Steel butt joint
 40000 psi
@Temperature 649 °C
Type 304 Stainless Steel butt joint
 50000 psi
@Temperature 427 °C
Type 304 Stainless Steel butt joint
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000293 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1742 °F
Solidus 1742 °FMelting Point
Liquidus 1742 °FFlow Point
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1745 - 1850 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd <= 0.0010 %
Carbon, C <= 0.0050 %
Gold, Au 81.5 - 82.5 %
Lead, Pb <= 0.0020 %
Nickel, Ni 17.338 - 18.45 %
Other, each <= 0.0010 %
Other, total <= 0.15 %
Phosphorus, P <= 0.0020 %
Zinc, Zn <= 0.0010 %
 
Descriptive Properties
ColorNickel Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy
AIM 95Sn/3.5Ag/1.5In Solder for Photonic Packaging
AIM 91Sn/9Zn Solder for Photonic Packaging
AIM 88Au/12Ge Solder for Photonic Packaging
AIM 80Au/20Sn Solder for Photonic Packaging

NLUCMI59 / 18126

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.