MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Total 3720Z Polypropylene, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: High flow reactor injection molding homopolymer

High Flow - FINA 3720Z has high flow characteristics that result in ease of filling thin wall parts.

Antistat - FINA 3720Z contains an antistat that will help protect molded parts from dust accumulation.

FDA - FINA 3720Z complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 3720Z is recommended for caps, closures, and thin wall containers.

Processing - FINA 3720Z resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 20 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D288A
Tensile Strength, Ultimate 33.1 MPaASTM D638
Elongation at Break 7.0 %ASTM D638
Modulus of Elasticity 1.45 GPaASTM D638
Flexural Modulus 1.17 GPaASTM D790
Izod Impact, Notched 0.267 J/cmASTM D256A
Izod Impact, Unnotched 10.65 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 121 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 232 °CInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pinnacle Polymers 1120 H Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
Total PPH 3720WZ Polypropylene, Injection Molding Grade
Petromont 1002 High Density Polyethylene Resin
Overview of materials for Polypropylene, Molded
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade

PFIN68 / 38398

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.