MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ThyssenKrupp FR-30® Fire Resistant Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: With the newly developed FR 30 fire resistant structural steel from TKS there is now the possibility, for the first time, to create steel structures with a fire resistance rating up to F30 without additional protection and without the otherwise customary fire protection precautions. It is possible to design structural components made from the FR steel in the unprotected condition, i.e. without any additional fire protection precautions, for fire exposure lasting up to 30 minutes (fire resistance rating F30) with extent-to-area ratios U/A = 60 to 100 m-1.

Information Provided by Thyssen Krupp

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 460 - 620 MPa66700 - 89900 psi
Tensile Strength, Yield >= 275 MPa>= 39900 psi
Elongation at Break 22 %22 %
Charpy Impact 27.0 J
@Temperature -20.0 °C
19.9 ft-lb
@Temperature -4.00 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr <= 0.85 %<= 0.85 %
Iron, Fe >= 96.7 %>= 96.7 %As Balance
Manganese, Mn <= 1.4 %<= 1.4 %
Molybdenum, Mo <= 0.40 %<= 0.40 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.015 %<= 0.015 %
Vanadium, V <= 0.060 %<= 0.060 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ThyssenKrupp XAR® 400 Structural Steel
ThyssenKrupp COR-TEN A Structural Steel
Overview of materials for AISI 6000 Series Steel
Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures
Industeel CREUSABRO® 4000 High Wear Resistant Steel

NTHYSS051 / 90371

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.