MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Fortron® FX530T4 PPS, Impact Modified, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

Material Notes: Product Description: Forton FX530T4 is a 30% glass filled, impact modified grade for injection molding with good thermal shock resistance.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber

Additive: Impact Modifier

Features: Impact Modified

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 21000 psiISO 527-2/5
Elongation at Break 2.0 %ISO 527-2/5
Tensile Modulus 1.45e+6 psiISO 527-1
Flexural Strength 29700 psiISO 178
Flexural Modulus 1.41e+6 psiISO 178
Charpy Impact, Notched 4.30 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 4.80 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 4.00e+9 ohm-cm
@Temperature 180 °C
IEC 62631-3-1
 >= 2.00e+14 ohm-cm
@Temperature 22.8 °C
IEC 62631-3-1
Surface Resistance >= 1.00e+11 ohm
@Temperature 22.8 °C
IEC 62631-3-2
 >= 1.00e+11 ohm
@Temperature 180 °C
IEC 62631-3-2
Dielectric Strength 530 V/mil
@Thickness 1850 mm
AC
 580 V/mil
@Thickness 9040 mm
AC
 860 V/mil
@Thickness 9040 mm
DC
 1000 V/mil
@Thickness 1850 mm
DC
Comparative Tracking Index 125 V100 drops; IEC 60112
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 86.0 °FHopper
 626 - 644 °FHot Runner
Feed Temperature 140 - 176 °FInjection
Rear Barrel Temperature 554 - 572 °F
Middle Barrel Temperature 590 - 608 °F
Front Barrel Temperature 626 - 644 °F
Nozzle Temperature 590 - 626 °F
Zone 4 626 - 644 °FInjection
Melt Temperature 626 - 644 °F
Mold Temperature 284 - 320 °F
Drying Temperature 266 - 284 °F
Dry Time 3.00 - 4.00 hour
Back Pressure <= 435 psi
Screw Speed 50 rpm
@Thickness 55.9 mm
 75 rpm
@Thickness 40.6 mm
 120 rpm
@Thickness 24.9 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6286 / 310979

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.