MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excellent cracking resistance regarding thermal shock. Rotors, magnetic coil coating This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS).

Processing: Injection and compression molding

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 - 1.95 g/cc1.85 - 1.95 g/ccISO 1183
Apparent Bulk Density 0.700 - 1.00 g/cc0.0253 - 0.0361 lb/in³ISO 60
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.10 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inInjection and Compression; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 - 120 MPa14500 - 17400 psiInjection and Compression; ISO 527
Modulus of Elasticity 15.0 - 18.0 GPa2180 - 2610 ksiInjection and Compression; ISO 527
Flexural Strength 190 - 210 MPa27600 - 30500 psiInjection and Compression; ISO 178
Flexural Modulus 16.0 - 19.0 GPa2320 - 2760 ksiInjection and Compression; ISO 178
Compressive Strength 200 - 220 MPa29000 - 31900 psiISO 604
Charpy Impact Unnotched 1.50 - 1.80 J/cm²7.14 - 8.57 ft-lb/in²Injection and Compression; ISO 179/1eU
Charpy Impact, Notched 0.400 - 0.600 J/cm²1.90 - 2.86 ft-lb/in²Injection and Compression; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cm1.00e+15 - 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 - 1.00e+15 ohm1.00e+14 - 1.00e+15 ohmIEC 60093
Dielectric Constant  4.0 - 6.0
@Frequency 100 Hz
4.0 - 6.0
@Frequency 100 Hz
IEC 60250
 4.0 - 6.0
@Frequency 1e+6 Hz
4.0 - 6.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 20.0 - 30.0 kV/mm508 - 762 kV/inIEC 60243-1
Dissipation Factor  0.010 - 0.020
@Frequency 100 Hz
0.010 - 0.020
@Frequency 100 Hz
IEC 60250
 0.020 - 0.040
@Frequency 1e+6 Hz
0.020 - 0.040
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 180 - 240 sec180 - 240 secASTM D495
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 50.0 - 150 °C
8.33 - 11.1 µin/in-°F
@Temperature 122 - 302 °F
ISO 11359-2
Thermal Conductivity 0.400 - 0.600 W/m-K2.78 - 4.16 BTU-in/hr-ft²-°FASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FISO 75-A
Deflection Temperature at 8.0 MPa 150 - 170 °C302 - 338 °FISO 75-C
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Shrinkage <= 0.050 %
@Temperature 110 °C,
Time 605000 sec
<= 0.050 %
@Temperature 230 °F,
Time 168 hour
Post shrinkage; ISO 2577
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature <=20.0 °C
6.00 Month
@Temperature <=68.0 °F
 
Descriptive Properties
Glow wire flammability test900/1IEC 60695 2-12
Glow wire ignitability test900/1IEC 60695 2-13
Water Absorption<10 mg24 hr, 23°C; ISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Raschig Group 3535 Epoxy
DIAB Divinycell® H 200 Sandwich Core Material
Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
Cosmic Plastics FARBOSET® 2460 All Colors Mineral Filled Epoxy Molding Compound
Cosmic Plastics E4920D Mineral Filled Epoxy Molding Compound

PRASCI06 / 179143

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.