MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Electrolytic (AAA) (Extra High Purity), Chill-Cast Tin
Categories: Metal; Nonferrous Metal; Tin Alloy; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.28 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 3.9
Tensile Strength, Ultimate 14.5 MPa
Modulus of Elasticity 49.9 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000126 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.5 µm/m-°C
Specific Heat Capacity 0.222 J/g-°C
Thermal Conductivity 66.8 W/m-K
Melting Point 231.9 °C
Boiling Point 2602 °C
 
Component Elements PropertiesOriginal ValueComments
Tin, Sn 99.98 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Electrolytic (AA) (High Purity), Chill-Cast Tin
68.4Pb-30Sn-1.6Sb Tin-Lead-Antimony Solder, ASTM Class 30C
Tin Grade A, Chill-Cast
96Sn-4Ag Tin-Silver Solder, ASTM Class 96TS, ISO/DIS 9453 Alloy 28
97Sn-3Ag Tin-Silver Solder, ISO/DIS 9453 Alloy 29

MLTN100 / 100298

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.