MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: ATI Ti-6Al-4V-ELI, Grade 23 alloy (Extra Low Interstitials, UNS R56407) is a higher purity grade of ATI Ti-6Al-4V alloy. This grade has lower oxygen, carbon, and iron content. It is used in biomedical applications such as surgical instruments, orthopedic implants, and is the preferred grade for marine and cryogenic applications, and some important aerospace components. This titanium grade is produced by vacuum arc primary melting followed by a second vacuum arc remelting operation.

Key Words: Ti 6-4; Titanium 6-4; ASTM B-265; ASTM F-136; ASME SB-265; AMS 4907-4; MIL-T-9046
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.43 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 30
Tensile Strength, Ultimate 828 MPa
Tensile Strength, Yield 759 MPa
@Strain 0.2 %
Elongation at Break 10 %
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 6.5 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.25 %
Nitrogen, N <= 0.030 %
Oxygen, O <= 0.13 %
Titanium, Ti 90 %as balance
Vanadium, V 4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V ELI (Grade 23), Annealed
Titanium Ti-6Al-4V (Grade 5), Annealed
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Titanium Ti-6Al-4V (Grade 5), STA
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age

NLTIT05E / 18056

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.