MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Polykemi AB POLYsan PN127 Styrene Acrylonitrile
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes:

Information provided by Polykemi AB

Key Words: Styrene Acrylonitrile
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break <= 70.0 MPaISO/R527
Elongation at Yield 6.0 %ISO/R527
Flexural Strength <= 124 MPaISO 178
Flexural Modulus 3700 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
ISO 179
 3.00 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C120°C/h; ISO 75/1
Vicat Softening Point 100 °C
@Load 5.001 kg
50°C/h; ISO 306
 106 °C
@Load 1.00 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Kibisan® PN107 SAN Resin, General Purpose
Ineos Nova 1504 High Heat Crystal Polystyrene
Chi Mei Polyrex® PG-80N Polystyrene
Chi Mei Polyrex® PG-383 Polystyrene
Chi Mei Kibisan® PN-107 L125 SAN

PPOLYK228 / 122953

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.