MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Extrusion 87758  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade; PVC, Sheet Grade

Material Notes: Finished part testing is required for ASTM E-84 certification. The Cell Classification was determined using the notched Izod test with injection molded samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.46 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81
@Time 15.0 sec
ASTM D2240
Tensile Strength, Yield 43.1 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2810 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 76.5 MPaASTM D790
Flexural Modulus 2940 MPaASTM D790
Izod Impact, Notched 90.7 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Flow, Compression Molded; ASTM D256A
 101 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 123 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Across Flow, Compression Molded; ASTM D256A
Dart Drop Total Energy 69.4 J/cm
@Temperature 23.0 °C
Procedure B, C.125 Dart; ASTM D4226
 69.4 J/cm
@Temperature 23.0 °C
Procedure A, C.125 Dart; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 67.8 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 188 - 199 °C
 
Descriptive Properties
Agency RatingsASTM E 84
FeaturesLow Smoke Emission
FormsPellets
Processing MethodSheet Extrusion
 Thermoforming
PVC Cell Classification13353ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH1PN8775 / 102611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.