MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast 8503-4/AboCure 8503-4 Colorless Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 8503-4/AboCure 8503-4 is a general purpose, moderate speed, colorless epoxy casting compound with low viscosity. It offers a convenient 2/1 ratio by volume and lends itself to casting of thicker layers than 8503-3, because of its slower reactivity. Suggested Uses: Transparent Casting, Embedding, Encapsulation, Potting, and Bonding. Casting display or experimental models without the high shrinkage of acrylic or other resins. Precise reproduction of anatomical or scientific models. Embedding organic, geologic, or metallurgic specimens. Encapsulation of electric, radioactive, or delicate components. Preservation or repair of artistic and historical objects. High-performance transparent table tops.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 500 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89
Tensile Strength at Break 9200 psi
Elongation at Break 14 %
Flexural Strength 14200 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 65.0 °CDeflection Temp at unknown load
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Pot Life 90 min
@Temperature 25.0 °C
500 g
 
Descriptive Properties
Hardening Time (min)120-720
Parts by Weight (pbw)100AboCast
 42AboCure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Devcon Zip Patch™ Epoxy
Devcon Underwater Repair Putty (UW) Epoxy
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste
Abatron AboCast/AboCure 8502-1 Epoxy

PABC890 / 107874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.