MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Daplen™ ED206HP TPO Compound
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polypropylene (PP); TPO

Material Notes: Daplen ED206HP is a 25% mineral reinforced compound intended for injection molding. ED206HP has been developed especially for the car industry, to be used in interior parts requiring excellent scratch resistance. ED206HP has good processability with optimized physical properties.

Daplen ED205HP has been developed especially for dashboards, interior panels, dashboard inserts, door panels and pockets, and consoles.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inBorealis Method
Melt Flow  7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 30 g/10 min
@Load 5.00 kg,
Temperature 230 °C
30 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ISO 868
Ball Indentation Hardness 35.0 MPa5080 psiH385/30; ISO 2039
Tensile Strength, Yield 20.0 MPa2900 psiAt 50 mm/min; ISO 527-2
Flexural Strength 20.0 MPa2900 psiISO 178
Flexural Modulus 1.92 GPa278 ksiAt 2 mm/min; ISO 527-2
Charpy Impact Unnotched NBNBISO 179/1eU
 6.20 J/cm²
@Temperature -20.0 °C
29.5 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.520 J/cm²
@Temperature -20.0 °C
2.47 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-2
Vicat Softening Point 56.0 °C133 °FB (50N); ISO 306
 135 °C275 °FA (10N); ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °F
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °F
 
Descriptive Properties
Emissions, ug C/g 24VDA 277
Fogging %98At 100°C/3 hours
Fogging, mg0.4At 100°C/ 16 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ ED135AI TPO Compound
Borealis Daplen™ AK4504 TPO Compound
Borealis Daplen™ ED213AE TPO Compound
Borealis Daplen™ EE040AE TPO Compound
Borealis Daplen™ EE103AE TPO Compound

PBOREA146 / 27453

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.