MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MAS Epoxies PENETRATING EPOXY SEALER Penetrating Epoxy Sealer Solvent-free System
Categories: Polymer; Thermoset; Epoxy

Material Notes: MAS Penetrating Epoxy Sealer is a 2:1 by volume ultra-low viscosity system designed to penetrate soft, rotten or damaged wood. Contains zero solvent for a VOC-free solution but add up to 50% solvent for more penetrating power. It restores strength and creates a stronger finished product. It can be used on window frames, door frames, windowsills, boat hulls, transom reinforcement and any other spongy or rotten wood. Ideal for sealing projects before coating or laminating applications to prevent warping due to temperature and humidity changes. Penetrates without any solvent for a VOC-free sealing solution, Excellent at repairing rotten wood for further repair, Seals wood and other substrates to prevent warping on woodworking projects.

Information provided by MAS Epoxies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 g/cc0.0351 lb/in³Hardener; ASTM D1475
 1.14 g/cc0.0411 lb/in³Resin; ASTM D1475
Viscosity 20 cP20 cPHardener; ASTM D2196
 150 cP150 cPInitial Mixed; ASTM D2196
 270 cP270 cPResin; ASTM D2196
 
Processing PropertiesMetricEnglishComments
Cure Time  2880 min
@Temperature 29.4 °C
48.0 hour
@Temperature 85.0 °F
Full cure
 5760 min
@Temperature 23.9 °C
96.0 hour
@Temperature 75.0 °F
Full cure
Tack-Free Time  360 - 480 min
@Temperature 29.4 °C
6.00 - 8.00 hour
@Temperature 85.0 °F
 600 - 720 min
@Temperature 23.9 °C
10.0 - 12.0 hour
@Temperature 75.0 °F
Gel Time  18.0 - 22.0 min
@Temperature 29.4 °C
18.0 - 22.0 min
@Temperature 85.0 °F
150g mass; ASTM D2471
 25.0 - 30.0 min
@Temperature 23.9 °C
25.0 - 30.0 min
@Temperature 75.0 °F
150g mass; ASTM D2471
 
Descriptive Properties
Mix Ratio by Volume2A : 1B
Mix Ratio by Weight100A : 43B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASZ905 / 265522

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.