Properties and applications: SIPERNAT represents a specific product range of precipitated silica, aluminum and calcium silicates. SIPERNAT 612 is a silica with neutral pH value and high absorption capacity used as a thickening agent. The silica has a medium particle size and a medium surface area.Information provided by Evonik |