MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for High Carbon Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "High Carbon Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.451 - 8.26 g/ccAverage value: 7.54 g/cc Grade Count:375
Particle Size 6.70 - 12.0 µmAverage value: 9.27 µm Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 163 - 600Average value: 260 Grade Count:235
Hardness, Knoop 195 - 769Average value: 297 Grade Count:177
Hardness, Rockwell B 43.0 - 100Average value: 95.7 Grade Count:176
Hardness, Rockwell C 10.0 - 70.0Average value: 46.4 Grade Count:284
Hardness, Vickers 182 - 748Average value: 286 Grade Count:177
Tensile Strength, Ultimate 161 - 3200 MPaAverage value: 1120 MPa Grade Count:269
Tensile Strength, Yield 275 - 3340 MPaAverage value: 896 MPa Grade Count:253
Elongation at Break 0.500 - 30.0 %Average value: 14.3 % Grade Count:242
Reduction of Area 13.4 - 73.0 %Average value: 38.7 % Grade Count:107
Modulus of Elasticity 13.8 - 235 GPaAverage value: 200 GPa Grade Count:338
Flexural Yield Strength 159 - 5130 MPaAverage value: 2260 MPa Grade Count:26
Compressive Yield Strength 1320 - 3100 MPaAverage value: 2160 MPa Grade Count:4
Bulk Modulus 160 GPaAverage value: 160 GPa Grade Count:188
Poissons Ratio 0.280 - 0.313Average value: 0.292 Grade Count:262
Fracture Toughness 13.2 - 165 MPa-m½Average value: 60.1 MPa-m½ Grade Count:5
Machinability 10.0 - 125 %Average value: 53.0 % Grade Count:152
Shear Modulus 78.0 - 82.7 GPaAverage value: 79.9 GPa Grade Count:264
Izod Impact 3.00 - 18.0 JAverage value: 8.90 J Grade Count:64
Izod Impact Unnotched 10.8 - 229 JAverage value: 53.5 J Grade Count:31
Charpy Impact 1.36 - 99.0 JAverage value: 34.1 J Grade Count:21
Charpy Impact, Unnotched 2.71 - 86.0 JAverage value: 19.2 J Grade Count:13
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.0000300 ohm-cmAverage value: 0.0000159 ohm-cm Grade Count:250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.90 - 14.8 µm/m-°CAverage value: 12.5 µm/m-°C Grade Count:219
Specific Heat Capacity 0.410 - 0.669 J/g-°CAverage value: 0.474 J/g-°C Grade Count:150
Thermal Conductivity 19.0 - 52.0 W/m-KAverage value: 45.9 W/m-K Grade Count:265
Maximum Service Temperature, Air 120 - 482 °CAverage value: 311 °C Grade Count:6
Transformation Temperature 183 - 910 °CAverage value: 593 °C Grade Count:63
 
Processing PropertiesOriginal ValueComments
Processing Temperature 168 - 1550 °CAverage value: 717 °C Grade Count:45
Annealing Temperature 740 - 900 °CAverage value: 826 °C Grade Count:12
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.0600 - 1.25 %Average value: 0.828 % Grade Count:6
Boron, B 0.000500 - 0.00300 %Average value: 0.00175 % Grade Count:40
Carbon, C 0.100 - 3.40 %Average value: 0.876 % Grade Count:366
Chromium, Cr 0.150 - 14.0 %Average value: 2.66 % Grade Count:264
Cobalt, Co 0.250 - 14.0 %Average value: 6.75 % Grade Count:21
Copper, Cu 0.100 - 0.350 %Average value: 0.300 % Grade Count:5
Iron, Fe 66.5 - 99.2 %Average value: 94.0 % Grade Count:366
Manganese, Mn 0.100 - 13.0 %Average value: 0.688 % Grade Count:348
Molybdenum, Mo 0.0600 - 10.5 %Average value: 1.34 % Grade Count:166
Nickel, Ni 0.100 - 10.0 %Average value: 0.955 % Grade Count:94
Phosphorus, P 0.0120 - 0.0500 %Average value: 0.0331 % Grade Count:272
Silicon, Si 0.100 - 2.20 %Average value: 0.345 % Grade Count:257
Sulfur, S 0.00100 - 0.270 %Average value: 0.0389 % Grade Count:286
Tungsten, W 0.150 - 13.0 %Average value: 4.36 % Grade Count:43
Vanadium, V 0.0700 - 14.5 %Average value: 2.53 % Grade Count:77

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
Overview of materials for Medium Carbon Steel
Overview of materials for Stainless Steel
Overview of materials for Low Alloy Steel
Overview of materials for Cast Iron

M01009 / 81720

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.