MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Flam™ 2702 PP Black Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Features:

  • Halogenated
  • Forms:

  • Pellets
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.06 g/ccASTM D792
    Linear Mold Shrinkage 0.012 cm/cmASTM D955
    Melt Flow 2.9 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Yield 2870 psiASTM D638
    Elongation at Break 930 %ASTM D638
    Flexural Strength 2730 psiASTM D790
    Flexural Modulus 101000 psiMethod I (3 point load), Procedure B); ASTM D790
    Izod Impact, Notched 14.0 ft-lb/inASTM D256
    Gardner Impact 15.83 ft-lbASTM D3029
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 1.30e+15 ohm-cmASTM D257
    Dielectric Strength 642 V/milASTM D149
     
    Thermal PropertiesOriginal ValueComments
    Flammability, UL94 V-2
    @Thickness 0.800 mm
     V-2
    @Thickness 3.00 mm

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    PMULTI293 / 54197

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.