Hostacom EKC 330N E1 G62514 is a 16% talc filled PP copolymer, with good flowability, excellent impact/stiffness balance, outstanding blooming resistance at elevated temperatures and good scratch resistance. This grade is delivered in G62514 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications: Automotive Parts, Interior TrimsInformation provided by LyondellBasell. |