MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives Metech 2232 Silver Conductor
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: This product is a silver bearing, thermoplastic, acrylic, polymer paint designed primarily as a conductive electrode solder base for tantalum capacitors. Additionally, this material can be used as a general purpose conductive paint for printed circuit board repair and electromagnetic shielding applications. It possesses good rheological properties for either dip or paint applications. The cured film has excellent electrical and environmental stability both initially and upon aging. The material is readily soldered using conventional tin/lead/silver solders for external lead attachment.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 350 - 450 cP350 - 450 cP
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 100 ohm<= 100 ohmDried at 80ºC for 10 minutes then cured at 150ºC for 30 minutes
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 40 - 44 %40 - 44 %
 
Descriptive Properties
Settling Rate (mm/hr)<=2
Solder Leach Resistance (cycles)>5Dried at 80ºC for 10 minutes then cured at 150ºC for 30 minutes; Tested in 62Sn/36Pb/2Ag solder at 205ºC
Solder Wetting (seconds)2-3Dried at 80ºC for 10 minutes then cured at 150ºC for 30 minutes; Tested in 62Sn/36Pb/2Ag solder at 205ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tantalum, UNS R05200
Tantalum, Ta; Cold Worked
Tantalum, Ta; Annealed
Abatron AboCoat 8508-1 Heavy-Duty Epoxy Paint

PLORD047 / 86055

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.