System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical LUSEP HI2402 PPS+GF40%, Injection Molding
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Sulfide (PPS)
;
Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Material Notes:
High impact
Application: Pump Units, Motor Units, etc..
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.60
g/cc
ASTM D792
Water Absorption
0.020 %
@Time 86400 sec
ASTM D570
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
175
MPa
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break
2.0 - 3.0 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Strength
260
MPa
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus
130000
kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched
11.7
kg-cm/cm
@Thickness 3.20 mm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
260
°C
@Thickness 6.40 mm
Unannealed; ASTM D648
Flammability, UL94
V-0
@Thickness 0.750 mm
Processing Properties
Original Value
Comments
Rear Barrel Temperature
300
°C
Middle Barrel Temperature
310
°C
Front Barrel Temperature
320
°C
Nozzle Temperature
330
°C
Melt Temperature
300
-
330
°C
Mold Temperature
120
-
150
°C
Drying Temperature
100
-
120
°C
@Time 7200 - 14400 sec
Moisture Content
<= 0.020 %
Screw Speed
<=
100
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LG Chemical LUSEP HI2302 PPS+GF30%, Injection Molding
LG Chemical LUSEP HI2202 PPS+GF20%, Injection Molding
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose
PLHCHEM9835 / 239351
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.