MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Carpenter Micro-Melt® HS-76 Alloy (AISI M48)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Micro-Melt® HS-76 alloy is a super high speed steel possessing abrasion resistance equal to T15 and superior red hardness to T15 and M42. It is heat treatable to HRC 70 and is a good candidate for special purpose cutting tools where the ASTM M40 series high speed steels are inadequate. The advantages of Micro-Melt premium powder high speed steels include ease of grinding, response to heat treatment, more uniform structure, greater wear resistance and improved toughness. In addition, Carpenter's unique hot rolling and rotary forging capabilities impart minimal distortion characteristics to these alloys.

Applications: Milling cutters, End mills, Cutting tool inserts, Extrusion die inserts, Lathe tools, Form tools, Broaches, Reamers, Cut-off tools

Information provided by Carpenter Technology Corporation.

Micro-Melt® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T11348
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.26 g/cc8.26 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 57 - 5957 - 59Tempered at 1200°F
 64 - 6664 - 66As quenched
Modulus of Elasticity 214 GPa31000 ksi
 
Thermal PropertiesMetricEnglishComments
Transformation Temperature 99.0 °C210 °FMS
 835 °C1540 °FAc1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.55 %1.55 %
Chromium, Cr 4.0 %4.0 %
Cobalt, Co 9.0 %9.0 %
Iron, Fe 66.44 - 66.5 %66.44 - 66.5 %As Balance
Manganese, Mn 0.20 %0.20 %
Molybdenum, Mo 5.25 %5.25 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.40 %0.40 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W 10 %10 %
Vanadium, V 3.1 %3.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C)
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar
Carpenter Custom 450® Stainless Steel, Annealed
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed

NCARN13 / 15852

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.