Notes: Medalist MD-12100 Series are high performance thermoplastic elastomer designed for use in healthcare and medical applications requiring high elasticity and excellent moldablity. Medalist MD-12140 is a low hardness, low density grade, available in NAT and colors, which can be sterilizable and exhibits excellent adhesion to polypropylene. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Sterilizable; Good Toughness; Halogen Free; Low Density; Low Flow; Low Hardness; Low Specific Gravity; Lubricated; Radiation Sterilizable; Radiation Resistant; Resilient; Slip; Without Fillers Uses: Bushings; Closures; Disposable Hospital Goods; Flexible Grips; Grommets; Knobs; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |