MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Danquinsa EMULTROL® E-77 H Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: EMULTROL E-77 H is a high quality, aqueous tackifier dispersion, which results in very good adhesion properties, even on non-polar substrates and polymer-bound cardboard surfaces. EMULTROL E-77 H is excellent compatible with acrylic resin dispersions, PVA, EVA, SBR, NBR and polyurethane. The product has good wetting properties on silicone paper and is highly stabilized against the effects of oxidation and the action of ultra-violet rays. The emulsion is comprised of extremely fine particles, therefore does not scratch application cylinders, and the product is highly stable during storage. The addition of additives with a high basic pH may cause the dispersion to become unstable. Equally, the addition of cationic substances should be avoided.

Application: The resin emulsion acts as modification component in one and two component aqueous adhesive and adhesive coating systems. This emulsion is added to different based aqueous plastic dispersions to achieve a permanent adhesiveness on bonding surfaces of the films. It is used as well to achieve a long open time. A typical application for this emulsion is for example the modification of aqueous primer dispersion adhesives for the coating of adhesive stripes, labels and film materials. We can specially recommend you EMULTROL E-77 H for adhesives, where it must be given a high hydrolysis and ageing resistance.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 - 1.03 g/cc0.0365 - 0.0372 lb/in³
pH 6.0 - 8.06.0 - 8.0
Viscosity <= 1500 cP<= 1500 cPRV8, Spindle 3, 50 rpm
Storage Temperature 10.0 - 25.0 °C50.0 - 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 50<= 50[mg KOH/g], residium
 
Thermal PropertiesMetricEnglishComments
Boiling Point 100 °C212 °F
Softening Point 74.0 - 78.0 °C165 - 172 °FResidue soft point
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Active matter contents53-55%
AspectWhitish liquid
CompositionHighly stable esterified rosin resin emulsion.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ173 / 294593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.