MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC LNP™ STAT-KON™ Compound RFD03 Polyamide 66 (Nylon 66) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP STAT-KON RFD03 compound is based on Nylon 6/6 resin containing conductive carbon powder and 15% glass fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
 0.620 %0.620 %23°C/50% RH/24 hrs; ASTM D570
 0.990 %0.990 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm0.010 - 0.030 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psi5 mm/min; ISO 527
 91.0 MPa13200 psi5 mm/min; ASTM D638
Tensile Strength, Yield 90.0 MPa13100 psi5 mm/min; ISO 527
 91.0 MPa13200 psi5 mm/min; ASTM D638
Elongation at Break 1.2 %1.2 %5 mm/min; ISO 527
 1.3 %1.3 %5 mm/min; ASTM D638
Elongation at Yield 1.2 %1.2 %5 mm/min; ISO 527
 1.3 %1.3 %5 mm/min; ASTM D638
Tensile Modulus 8.01 GPa1160 ksi1 mm/min; ISO 527
 8.92 GPa1290 ksi50 mm/min; ASTM D638
Flexural Strength 134 MPa19400 psiISO 178
 177 MPa25700 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 179 MPa26000 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.33 GPa918 ksi1.3 mm/min, 50 mm span; ASTM D790
 6.60 GPa957 ksi2 mm/min; ISO 178
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
Izod Impact, Unnotched 2.91 J/cm5.45 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 5.00 J3.69 ft-lbASTM D3763
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10 ohm - 1e+0510 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 3.00 µm/m-°C
@Temperature -30.0 - 30.0 °C
1.67 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 8.00 µm/m-°C
@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 258 °C496 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 258 °C
@Thickness 3.20 mm
496 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 247 °C
@Thickness 3.20 mm
477 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 295 °C536 - 563 °F
Zone 3 295 - 305 °C563 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 95.0 - 110 °C203 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81370 / 289317

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.