MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carlson C 800AT Nickel-Iron-Chromium Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: General Description

Carlson Alloy C 800AT is a modification of Carlson Alloy C 800, exhibiting higher creep and rupture strengths. This nickel-iron-chromium alloy has a carbon content restricted to a range of 0.06 to 0.10%. The aluminum plus titanium content of this alloy is also maintained in the upper portion of the standard range (0.85 to 1.20%).

C 800AT is solution-annealed at 2100°F (1500°C). That heat treatment and the compositional restrictions are responsible for this alloy’s improved creep and rupture strengths.

Since the chemistry of C 800AT falls within the range of C 800, there are no significant differences in physical and thermal properties. The major differences between the alloys are in the mechanical properties. (Generally C 800 exhibits higher mechanical properties at room temperature and during short-term exposure to elevated temperatures.) C 800AT displays superior and rupture strengths over long-term exposure to elevated temperatures.

C 800AT offers higher ASME boiler and pressure vessel design stress allowables in creep and rupture test ranges than C 800H.

Applications

  • Chemical and Petrochemical – piping, tubing, pigtails and outlet manifolds in steam/hydrocarbon reforming; tubing for ethylene production; tubing and heaters for oxo-alcohol production; hydrodealkylation units; tubing, flanges and bends for production of vinyl chloride monomer.
  • Thermal Processing – tubing, muffles, retorts and fixtures in heat treating furnaces.
  • Power Generation – tubing in power plant superheaters and reheaters.

Information provided by Carlson

Key Words: UNS N08811
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.287 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 65000 psi
Tensile Strength, Yield >= 25000 psi
@Strain 0.2 %
Elongation at Break >= 30 %
Modulus of Elasticity 28500 ksi
Poissons Ratio 0.339
Shear Modulus 73.6 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1.014200 Oersted
Curie Temperature -115 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.2 µin/in-°F
@Temperature 21.1 - 871 °C
Melting Point 2475 - 2525 °F
Solidus 2475 °F
Liquidus 2525 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.15 - 0.60 %
Carbon, C 0.060 - 0.10 %
Chromium, Cr 19 - 23 %
Copper, Cu <= 0.75 %
Iron, Fe >= 39.5 %
Manganese, Mn <= 1.5 %
Nickel, Ni 30 - 35 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.015 %
Titanium, Ti 0.15 - 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed
ASTM A285, Grade C
ASTM A562 Carbon Steel, Titanium Alloy
ASTM A516, Grade 60
ASTM A516, Grade 55

NCARLSO23 / 15830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.