Description: HexPly® M79 is a hotmelt, thermosetting, low-exothermic epoxy resin matrix, specifically designed for prepreg applications at which short cure cycles below 100°C are required. M79 can be used for manufacture of large industrial components, suitable for cure of thin and thick sections. M79 exhibits a long out-life of 8 weeks at ambient conditions. M79 is supplied as moderate tack resin matrix.Information provided by Hexcel Corporation. |