Notes: MDF4 is a 15% glass fiber reinforced nylon 6 that offers improved mechanical performance coupled with good surface finish. Availability: Europe; North America Fillers/Reinforcement: Glass Fiber, 15% Filler by Weight Features: Good Surface Finish Processing Method: Injection Molding Information provided by Teknor Apex |