BVC 1204-70 Clear has been designed as a general purpose extrusion compound for use in spiral hose, window profiles and applications where high gloss is required. This material offers excellent extrusion characteristics as well as adhesion to rigid properties. It also contains a UV stabilizer for light and heat stability.Information Provided by Bayshore Vinyl Compounds Inc., a Mexichem Company. |