MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mi-Tech Metals HD18 Tungsten-Based Metal
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.

Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduces soldering or erosion problems. To increase the machinability of this brittle metal, alloying elements are added and practical use of tungsten is possible for die casting tools.

Used in resistance brazing and high temp applications. Used as counter weights and counter balances, radiation shielding components, tool shanks for boring bars and other tools for chatter-free machining.

Data provided by Mi-Tech Metals.

Key Words: Class 3 Tungsten Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 18.0 g/cc0.650 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 3434
Tensile Strength, Ultimate 758 MPa110000 psi
Tensile Strength, Yield 590 MPa
@Strain 0.2 %
85600 psi
@Strain 0.2 %
Elongation at Break 7.0 %7.0 %in 50 mm
Modulus of Elasticity 310 GPa45000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000110 ohm-cm0.0000110 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.43 µm/m-°C
@Temperature 20.0 - 400 °C
2.46 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity 138 W/m-K958 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 1.5 %1.5 %
Nickel, Ni 3.5 %3.5 %
Tungsten, W 95 %95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Beryllium Copper, UNS C17000
Mi-Tech Metals HD18.5 Tungsten-Based Metal
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
AK Steel ASTM A 715 Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)

NMITECH29 / 18439

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.