MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Medalist® MD-50168 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-50100 Series of medical-grade TPEs can be used as an alternative to flexible PVC and silicone in face masks used in respiratory therapy. Medalist MD-50168 is a medium hardness, low density, RoHS compliant grade that can be sterilized and is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Sterilizability; Good Toughness; Halogen Free; High Flow; Low Density; Low Specific Gravity; Medium Hardness; No Animal Derived Components; Radiation (Gamma) Resistant; Resilient; Slip; Without Fillers

Uses: Disposable Hospital Goods; Handles; Knobs; Medical Devices; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.885 g/cc0.0320 lb/in³ASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  67
@Time 5.00 sec
67
@Time 0.00139 hour
Injection Molded; ASTM D2240
 70
@Time 1.00 sec
70
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 10.3 MPa1490 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain  2.14 MPa
@Strain 50 %
310 psi
@Strain 50 %
Die C, 20 in/min; ASTM D412
 2.52 MPa
@Strain 100 %
365 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 3.96 MPa
@Strain 300 %
575 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 700 %700 %Die C, 20 in/min; ASTM D412
Tear Strength 45.6 kN/m260 pliFlow, Die C, 20 in/min; ASTM D624
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
23 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 350 °F
Middle Barrel Temperature 182 - 204 °C360 - 400 °F
Front Barrel Temperature 193 - 216 °C380 - 420 °F
Nozzle Temperature 182 - 227 °C360 - 440 °F
Melt Temperature 182 - 227 °C360 - 440 °F
Mold Temperature 26.7 - 48.9 °C80.0 - 120 °F
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 1.27 cm0.150 - 0.500 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-12160H Thermoplastic Elastomer
Teknor Apex Medalist® MD-17270 Thermoplastic Elastomer
Teknor Apex Medalist® MD-160 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12362 Thermoplastic Elastomer
Teknor Apex Medalist® MD-50357 Thermoplastic Elastomer

PTEKNQ0731 / 237222

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.