MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Von Roll Vetronite® G-11 Epoxy-Glass Fabric Laminate
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Highlights: Excellent mechanical properties at high temperatures, high CTI, EN 45545 approved.

Glass fabric laminates are manufactured using high-pressure techniques and are characterized by extremely high mechanical strength and outstanding electrical and thermal properties. All Vetronite® laminates are made of glass fabric bonding with an appropriate resin system.

Information provided by Von Roll.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccISO 1183
Water Absorption 0.040 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 375 MPaISO 527
Flexural Strength 350 MPa
@Temperature 150 °C
flatwise; ISO 178
 550 MPa
@Temperature 23.0 °C
flatwise; ISO 178
Compressive Strength 620 MPaflatwise; ISO 604
Charpy Impact, Notched 75.0 kJ/m²Edgewise; ISO 179
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.00e+18 ohmafter immersion in water; IEC 60167
Dielectric Strength 20.0 kV/mmflatwise; IEC 60243-1
Dielectric Breakdown 80000 VTaper pin electrodes, edgewise; IEC 60243-1
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°CDIN 53752
Maximum Service Temperature, Air 180 °CTemperature Index; IEC 60216
 
Descriptive Properties
ColorYellow Brown
ReinforcementGlass fabric
Sheet Sizes (mm)4250 x 1255, 2070 x 1070, 1170 x 1070

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVONR9912 / 249202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.