MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hardwire 3SX-4-12 Low Density Composite
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Metal Foam, Mesh, or Honeycomb

Material Notes: The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as well as better handling characteristics than the 3S. The 3SX wire cord is made by twisting three identical wire filaments (All filaments are 0.0189 in diameter) together at a longer than usual lay length and then over-wrapping the bundle with a single filament. The result is a cord with lower twist angles and straighter filaments that is the basis for the increased compressive strengths.

Characteristics:

  • 3SX tapes have the highest compressive strengths of all Hardwire tapes and tend to match or exceed the tensile properties.
  • Increased mechanical bonding in resins.
  • Better interlaminar shear resistance.
  • The cords do not bloom in failure modes during compression or tension.
  • Laminates exhibit steel like characteristics with high ductility and extreme deflection capability.
  • Very high flexural strength as well as ductile failure modes (laminates tend to bend – not break).
  • The best tape for bending angles and can be done in standard sheet metal breaks.
  • Very boardy feel – excellent for flat surfaces but still conformable enough for curved structures.
  • Better handling characteristics and cutability than 3S tapes.

All information provided by Hardwire, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0528 lb/in³Laminate Density
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 16.5 GPa2400 ksiEffective Modulus
Flexural Yield Strength 159 MPa23000 psiSheet Stress

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ERG Aerospace Duocel® Aluminum Metal Foam
Cymat A35620SC 020SS Stabilized Aluminum Foam
Cymat A35620SC 030SS Stabilized Aluminum Foam
FiberNide Nickel Aluminide Foam Atomic 22% Aluminum
Hexcel® HexWeb® CR III 1/8-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb

NWIRE02 / 19988

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.