System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LATI Latan 13E71 POM
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, Unreinforced
Material Notes:
Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.34
g/cc
0.0484
lb/in³
Linear Mold Shrinkage, Flow
0.023
-
0.027
cm/cm
0.023
-
0.027
in/in
Linear Mold Shrinkage, Transverse
0.0235
-
0.0275
cm/cm
0.0235
-
0.0275
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
35.0
MPa
5080
psi
Elongation at Break
>= 100 %
@Temperature 60.0 °C
>= 100 %
@Temperature 140 °F
>= 100 %
@Temperature 90.0 °C
>= 100 %
@Temperature 194 °F
100 %
@Temperature 23.0 °C
100 %
@Temperature 73.4 °F
Tensile Modulus
0.500
GPa
@Temperature 90.0 °C
72.5
ksi
@Temperature 194 °F
0.900
GPa
@Temperature 60.0 °C
131
ksi
@Temperature 140 °F
1.50
GPa
@Temperature 23.0 °C
218
ksi
@Temperature 73.4 °F
Charpy Impact Unnotched
NB
NB
Charpy Impact, Notched
1.00
J/cm²
4.76
ft-lb/in²
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
65.0
°C
149
°F
Deflection Temperature at 0.46 MPa (66 psi)
145
°C
293
°F
Deflection Temperature at 1.8 MPa (264 psi)
65.0
°C
149
°F
Vicat Softening Point
125
°C
@Load 5.00 kg
257
°F
@Load 11.0 lb
Processing Properties
Metric
English
Comments
Melt Temperature
175
-
200
°C
347
-
392
°F
Mold Temperature
60.0
-
90.0
°C
140
-
194
°F
Drying Temperature
80.0
-
90.0
°C
@Time 10800 sec
176
-
194
°F
@Time 3.00 hour
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LATI Latan 9 POM
LATI Latan 3E71 POM
LATI Latan 23UVE71 POM
LATI Latan 23UV POM
LATI Latan 2 POM
PLATH9751 / 177447
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.