HyTemp NPC50 is a 50% active dispersion of a quaternary ammonium salt in an ACM elastomer binder. NPC50 functions as an accelerator with sodium stearate in HyTemp 4050 series elastomers. NPC50 provides extremely fast property development, excellent shelf stability and good scorch safety up to 100°C. This product is supplied as light blue pellets dusted with clay to prevent agglomeration.Information provided by Zeon Chemicals. |