MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 6 GF 40 Polyamide 6, 40% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Features

PA 6 for injection moulding, chemically strengthened with 40% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electro tools, hobby tools, gears, covers of electric appliances, cooling screws of blowers, electromotors, carrying parts in the automotive industry. Delivered in natural mode and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccSTN 64 0111
Linear Mold Shrinkage 0.0152 cm/cmSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0148 cm/cmSTN 64 0808
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 210 MPaSTN EN ISO 527-2
Elongation at Break 2.0 %STN EN ISO 527-2
Tensile Modulus 13200 MPaSTN EN ISO 527-2
Flexural Strength 290 MPaSTN EN ISO 178
Flexural Modulus 11000 MPaSTN EN ISO 178
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 90.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 14.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 210 °CSTN EN ISO 75/A
Vicat Softening Point 210 °CB; STN EN ISO 306
Flammability, UL94 HB
Glow Wire Test 650 °CSTN IEC 60695-2-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 280 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %STN EN ISO 960
Injection Pressure 90.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® HTN51G35HSLR BK420 PA6T/XT-GF35
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled
Adell AD-30 Nylon 66, Ultra High Impact
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry)

PPLACO012 / 106890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.