MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KaMin Lithosperse® 7005CS Kaolin Clay - Surface Treated
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Lithosperse® 7005 CS is a high performance treated kaolin designed to improve rheology with outstanding dispersibility and resistance to clay bleed in lithographic cold set inks. Lithosperse® 7005 CS has been designed for mix, pump and filter production systems to minimize filter plugging.

Industry: Ink

Uses: Lithographic/Offset, Sheetfed, Web Offset Heatset, Web Offset Coldset, Letterpress

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brightness 84 %Reflectance (TAPPI)
Oil Absorption 40 %
Moisture Absorption at Equilibrium <= 1 %As Produced
Particle Size 0.40 µmAverage Stokes Equivalent Diameter
 
Descriptive Properties
CAS Number1332-58-7
Crystalline Silica (quartz)<0.1%
Physical FormDry
Shipping PointMacon, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kaolinite (Al2O3-2SiO2-2H2O)
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness
KaMin Polyfil® WC-426 Kaolin Clay - Calcined
KaMin Polyfil® 70 Kaolin Clay - Calcined
KaMin Kamintex® D Kaolin Clay - Calcined, high solids

CKAMAN926 / 178397

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.