MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bayshore Vinyl Compounds BRC R409002 Molding Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: BRC 409002 is a medium impact high flow injection molding compound designed for ease of process along with excellent weathering characteristics.

Information Provided by Bayshore Vinyl Compounds Inc., a Mexichem Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D2240
Tensile Strength at Break 5800 psiASTM D638
Tensile Modulus 370 ksiASTM D638
Flexural Yield Strength 10.6 ksiASTM D790
Flexural Modulus 380 ksiASTM D790
Izod Impact, Unnotched 15.0 ft-lb/inASTM D256
Impact 3.8Gardner [in-lb/mil]; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 65.0 °CASTM D648
 
Descriptive Properties
Equilibrium Torque (metergrams)1000187°C, 65g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary PVC 2235RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic
Colorite Polymers Flexchem 3551-02 Vinyl Compound
Dow AFFINITY™ SM 1300 Polyolefin Plastomer
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound
Bayshore Vinyl Compounds BVC 1100-78 Clear PVC Compound

PBAYS010 / 93282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.