MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Biomedical BioSpan® S SPU Segmented Polyether Polyurethane (SPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.

The combination of properties inspires exceptional devices In addition to excellent flex life, BioSpan® SPU offers a combination of additional properties, including low modulus, high tensile strength, high elongation, proven biocompatibility and good biostability. Because of these properties, it is used in ventricular assist devices as well as in artificial hearts, interventional cardiology balloons, drug eluting stents and spinal implants.

Tailor Made BioSpan® SPU can be enhanced with SME® technology to incorporate different surface active end groups such as silicone and fluorocarbon. SME® technology eliminates the need for additional surface modification steps after the device component is fabricated.

Summary of Product Benefits

  • Excellent flex life
  • Outstanding mechanical strength
  • Hydrolytically stable
  • Extremely elastic
  • Biocompatible
  • Adaptable with SME® technology
  • Comprehensive FDA Master File

Information provided by DSM Biomedical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 1.08 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 5600 psiASTM D1708
Elongation at Break 847 %ASTM D1708
Modulus of Elasticity 1.504 ksiinitial; ASTM D1708
Coefficient of Friction 6.4ASTM D1894
 
Descriptive Properties
Ames Mutagenicity AssayNon-mutagenic
AppearanceTranslucent
Balb/c-3T3 Cell TransformationDoes not induce morphological cell transformation in activated or non-activated test systems
Chromosome AberrationNon-genotoxic
Contact Angle (°)94
HemolysisNon-hemolytic
Intracutaneous InjectionNon-toxic
Kligman’s Maximization-CSO extractWeak allergic potential
Kligman’s Maximization-NaCl extractWeak allergic potential
Lee White ClottingNo effect on the clotting time of whole blood
Primary MucosalNon-irritant
Primary SkinNon-irritant
Repeat Dose IV StudyNon-toxic
Solution Concentration by Weight (%)20
USP Acute SystemicNon-toxic
USP Cytotoxicity (MEM Elution)Non-cytotoxic
USP Muscle Implantation (120 days/rats)Macroscopic-not significant tissue contact irritation, Microscopic-slight irritant
USP Muscle Implantation (14 days/rats)Macroscopic-not significant tissue contact irritation, Microscopic-Non-irritant
USP PyrogenNon-pyrogenic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DSM Biomedical BioSpan® F SPU Segmented Polyether Polyurethane (SPU)
DSM Biomedical BioSpan® SPU Segmented Polyether Polyurethane (SPU)
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
DSM Biomedical PurSil® 10 Thermoplastic Silicone Polyether Urethane
DSM Biomedical Bionate® 80A Thermoplastic Polycarbonate Polyurethane (PCU)

PBIOS001a / 138517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.