Data provided by the manufacturer, Exxon Chemical. A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through type packaging equipment. Film produced from LD-117 can be drawn down to 1.0 mil gauge. Applications: Bakery product overwrap; Soft goods (paper products) overwrap; Film is particularly suitable for applications requiring stiffness, crispness, machinability and abrasion resistance. Data for film properties below based on 1.5 mil film. |
Medium Density Polyethylene; Exxon Chemical Company |