MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3270 Polypropylene Homopolymer, High Crystallinity, Low Melt Flow Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Low Residuals TOTAL Polypropylene 3270 utilizes the TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.

Slip/Antiblock. 3270 is available with custom slip and antiblock packages

FDA. 3270 complies with all applicable FDA regulations for food contact use.

Recommended Applications. TOTAL Polypropylene 3270 is recommended in orientation processes for manufacture of packaging tapes and films that benefit from improved stiffness and barrier protection.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D1505
Water Vapor Transmission 0.200 g/100 in²/day
@Temperature 37.8 °C
90% RH; ASTM F1249-90
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 150 %ASTM D882
Film Elongation at Break, TD 60 %ASTM D882
Film Tensile Strength at Break, MD 28000 psiASTM D882
Film Tensile Strength at Break, TD 39000 psiASTM D882
1% Secant Modulus, MD 420000 psiASTM D882
1% Secant Modulus, TD 700000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ASTM D1003
Gloss 85 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 450 - 525 °FOriented Film Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications
Ineos H35Z-00 Polypropylene Homopolymer
Total PPH M3766 Metallocene Isostatic Polypropylene Polymer, Fiber Grade
Total PPR 8473 Polypropylene, Film Extrusion Grade
Total PPH 7069 Polypropylene, Homopolymer

PTOTAL811 / 130536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.