MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lanxess LEWATIT® MonoPlus M 500 KR Ion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus M 500 KR is a strongly basic, premium grade, gel-type anion exchange resin (type I) with beads of uniform size (monodisperse) in highly regenerated from (min 95% OH) and purified (extremely low content of desorbable chloride ions) to meet nuclear industry specifications. Lewatti nuclear resins (Lewatit KR) are noted for their outstanding mechanical and chemical stability and their high osmotic stability. Because of their excellent hydrodynamic behavior Lewatit KR resins allow particularly high flow rates. The extremely high monodispersity (uniformity coefficient: max 1.1) and very low fines content of max 0.1% (<0.315 mm) result in particularly low pressure losses compared with standard resins. Used in radioactive water circuits they provide a number of special tasks and guarantee a water quality that fully complies with the requirements of the nuclear power industry. Lewatit MonoPlus M 500 KR is particularly suitable for the:
  • removal of anions, including radioactive isotopes, from aqueous solutions (including boric acid)
  • decontamination of circuits in nuclear reactor plants
  • treatment of primary coolant e.g. in pressure water reactors
  • purification of steam generator blow down irrespective of the conditioning with Levoxin (hydrazine), ethanolamine or morpholine
  • polishing in the primary and secondary sections as a mixed bed component with Lewatit MonoPlus SP 112 KR or Lewatit MonoPlus 200 KR.

    Important! Rinse carefully with demineralized water prior to service or mixing with Lewatit MonoPlus SP 112 KR or Lewatit MonoPlus S 200 KR.

    Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.690 g/cc0.0249 lb/in³
Density 1.07 g/cc0.0387 lb/in³
Bead Size 0.590 - 0.690 mm0.0232 - 0.0272 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0040 %0.0040 %40 mg/kg
Calcium, Ca 0.0050 %0.0050 %50 mg/kg
Cobalt, Co 0.0010 %0.0010 %10 mg/kg
Copper, Cu 0.0010 %0.0010 %10 mg/kg
Iron, Fe 0.0050 %0.0050 %50 mg/kg
Lead, Pb 0.0010 %0.0010 %10 mg/kg
Mercury, Hg <= 0.00010 %<= 0.00010 %<1 mg/kg
Potassium, K 0.0020 %0.0020 %20 mg/kg
SiO2 0.010 %0.010 %100 mg/kg
Sodium, Na 0.0020 %0.0020 %20 mg/kg
 
Descriptive Properties
AppearanceLight brown, translucent
pH Operating Range0 - 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8777 / 209169

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.