MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aluminum Castings

(Viewing data as-entered. Click here to return)
Aluminum 222.0-T61, Sand Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Key Words: Aluminium 222.0-T61; UNS A02220; AA222.0-T61; Al222.0-T61
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.95 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 100 - 130AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 144Estimated from Brinell Hardness.
Hardness, Rockwell A 45Estimated from Brinell Hardness.
Hardness, Rockwell B 72Estimated from Brinell Hardness.
Hardness, Vickers 130Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 30.0 ksiAA
Tensile Modulus 71.0 GPaEstimated
Poissons Ratio 0.33Estimated
Machinability 90 %0-100 Scale (100=best)
Shear Modulus 26.7 GPaEstimated
Shear Strength 127 MPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000520 ohm-cmAA; Typical 33% IACS Conductivity
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 12.3 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical
 13.1 µin/in-°F
@Temperature 20.0 - 300 °C
AA; Typical; average over range
Specific Heat Capacity 0.963 J/g-°CTypical for cast aluminum
Thermal Conductivity 0.310 cal cm/sec-cm²-°CAA; Typical at 25°C
Melting Point 965 - 1155 °FAA; Typical
Solidus 965 °FAA; Typical
Liquidus 1155 °FAA; Typical
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 84 %As remainder
Copper, Cu 9.2 - 10.7 %
Iron, Fe 1.5 %
Magnesium, Mg 0.15 - 0.35 %
Manganese, Mn 0.50 %
Nickel, Ni 0.50 %
Silicon, Si 2.0 %
Titanium, Ti 0.25 %
Zinc, Zn 0.80 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 222.0-O, Sand Cast
Aluminum 201.0-T4, Sand Cast
Aluminum 204.0-T6, Sand Cast, Precipitation Treatment 12 h at 180°C (360°F)
Aluminum 242.0-O, Sand Cast
Aluminum A356.0-T6, Sand Cast

MAC2220T61 / 9797

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.