MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Novodur® P2H-AT Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Novodur® P2H-AT is a general purpose injection molding grade providing high flowability and contains an antistatic additive. High flowability, Good stiffness, High gloss. Applications: Household appliances, Sport articles, Oven casings.

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 37 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 110 MPaISO 2039-1
Tensile Strength, Yield 44.0 MPaISO 527
Elongation at Break >= 15 %ISO 527
Elongation at Yield 2.1 %ISO 527
Tensile Modulus 2500 MPaISO 527
Flexural Strength 70.0 MPaISO 178
Flexural Modulus 2400 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 16.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 16.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mmShort time, 1.5 mm; IEC 60243-1
Dissipation Factor 0.0055
@Frequency 100 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 98.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 260 °CISO 294
Mold Temperature 60.0 - 80.0 °CISO 294
Injection Velocity 240 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Delrin® SC699 NC010 POM
Covestro Makrolon® 2205 Polycarbonate, Injection Grade
Covestro Bayblend® T65 XF Polycarbonate + ABS
Covestro Bayblend® T45 Polycarbonate + ABS
Covestro Bayblend® T45 PG Polycarbonate + ABS

PSTYR9809 / 216036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.