MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mateck Potassium Bromide (KBr)
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.75 g/cc0.0994 lb/in³
Solubility 53.48 ppm53.48 ppm
a Lattice Constant 6.598 Å6.598 Å
c Lattice Constant 6.598 Å6.598 Å
Molecular Weight 119.01 g/mol119.01 g/mol
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 100100MPa
Hardness, Mohs 1.51.5
Modulus of Elasticity 13.8 GPa2000 ksiin <110> direction
 33.0 GPa4790 ksiin <100> direction
Poissons Ratio 0.1380.138
Shear Modulus 5.10 GPa740 ksiin <110> direction
 9.00 GPa1310 ksiin <100> direction
 
Thermal PropertiesMetricEnglishComments
CTE, linear 36.6 - 39.6 µm/m-°C
@Temperature -60.0 - 60.0 °C
20.3 - 22.0 µin/in-°F
@Temperature -76.0 - 140 °F
Specific Heat Capacity 0.4522 J/g-°C0.1081 BTU/lb-°F
Thermal Conductivity 4.81 W/m-K
@Temperature 46.0 °C
33.4 BTU-in/hr-ft²-°F
@Temperature 115 °F
Melting Point 728 °C1340 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.52511.5251n10.6
 1.4253
@Wavelength 30000 nm
1.4253
@Wavelength 30000 nm
 1.5319
@Wavelength 6000 nm
1.5319
@Wavelength 6000 nm
 1.5639
@Wavelength 546.1 nm
1.5639
@Wavelength 546.1 nm
at ne
 1.57
@Wavelength 500 nm
1.57
@Wavelength 500 nm
 2.0995
@Wavelength 200 nm
2.0995
@Wavelength 200 nm
Transmission, Visible 98 %
@Wavelength 500 nm
98 %
@Wavelength 500 nm
Internal Transmittance
IR Transmittance  26 %
@Wavelength 30000 nm
26 %
@Wavelength 30000 nm
Internal Transmittance
 98 %
@Wavelength 15000 nm
98 %
@Wavelength 15000 nm
Internal Transmittance
UV Transmittance 48 %
@Wavelength 200 nm
48 %
@Wavelength 200 nm
Internal Transmittance
 
Descriptive Properties
Cleavability(100)perfect
Constants of Elastic Compliance (Pa^-1)1.9492E-10S44
 3.029E-11S11
 -4.18E-12S12
Symmetrycubic
Symmetry Classm3m
Thermal Coefficient of Refractive Index-3.95E-5 to -4.29E-5at 3.39 microns for ± 60°C
Transmission Range (microns)0.21 - 28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mateck Sodium Chloride (NaCl)
Sodium Bromide, NaBr
Lead (II) Sulfide, PbS
Lead Telluride, PbTe (Altaite)
Lead Sulfide, PbS (Galena)

CMAT049 / 87733

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.