MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EC477AA Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: WESTLAKE polyethylene EC477 is a low-density resin designed for applications where high coating speeds and good drawdown are required. This material demonstrates good adhesion to paper, provides a good moisture barrier, and is heat-sealable at low temperatures.

    Application/Uses
  • Medium and lightweight coatings and laminations
  • Substrate coatings to provide heat sealability
  • Hot melt laminating adhesive
  • General purpose coatings

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Good adhesion to paper, provides a good moisture barrier, and is heat-sealable at low temperatures
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccASTM D1505
Melt Flow 16 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1300 psiASTM D638
Elongation at Break 450 %ASTM D638
 
Processing PropertiesOriginal ValueComments
Melt Temperature 575 - 625 °F
 
Descriptive Properties
ProcessCoating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake LF 2032 LLDPE
Westlake HM 5004 High Density Polyethylene
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
Westlake EC476AA Low Density Polyethylene

PWESF037 / 84474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.